Labradorite |
| |
Physical & mechanical properties
|
| |
Volumetric weight: | -
| |
Water absorbtion: | 0.03-0.18 %
| |
Compression strength: | 171 MPa
| |
Flexure strength: | -
| |
Attritive ability of rock: | 0.71 g/cm²
|
 |
Minerals (%)
| |
Pyroxene: | 3-7
| |
Plagioclase: | 85-93
| |
Olivine: | 1-3
| |
Biotite: | <1
| |
Others: | -
|
 |
|
 |
 |
 |
Deposit name: Verkholuzhske
Zhitomir region
|
|
 |
|